Tipo: article
Título: Biocompatibility of RealSeal, its primer and AH Plus implanted in subcutaneous connective tissue of rats
Autor(es): Grecca, Fabiana Soares
Kopper, Patrícia Maria Poli
Santos, Régis Burmeister dos
Fossati, Anna Christina Medeiros
Carrard, Vinícius Coelho
Acasigua, Gerson Arison Xavier
Figueiredo, José Antônio Poli de
Editor: Faculdade de Odontologia de Bauru
Fecha de Publicación: 2011
Volumen: 19
Primera página: 52
Última página: 56
Palabras clave: BIOCOMPATIBLE MATERIALS
ROOT CANAL FILLING MATERIALS
SUBCUTANEOUS TISSUES
ENDODONTICS
ODONTOLOGIA
ENDODONTIA
Resumen: Objective: This study tested rat connective tissue response to RealSeal, RealSeal primer or AH Plus after 7, 15, 30, 60 and 90 days of implantation. Material and methods: Thirty Wistar rats had subcutaneous sockets created on their back and received four implants each of polyethylene tubes containing one of the materials tested according to the groups: AH (AH Plus Sealer); RS (RealSeal Sealer); RP (RealSeal Primer); CG (control group – empty tube). After histological processing, sections were analyzed to identify the presence of neutrophils, lymphocytes and plasma cells, eosinophils, macrophages and giant cells, as well as fibrous capsule and abscesses, by an examiner using ligth microscope. Kruskal-Wallis and multiple comparisons test were used for statistical analysis. Significance level was set at 5%.Results: Lymphoplasmacytic infiltrate scores significantly higher than of the control group were observed at 14 and 60 days in AH group, and at 90 days in RS group (p<0.05). There were no differences in terms of presence of macrophages, giant cells, eosinophils, neutrophils and fibrosis. AH Plus group scored higher for abcesses at seven days than any other period (p=0.031)RP group scored higher for lymphoplasmacytic infiltrate at 14 days than at 90 days. Conclusion:The main contribution of this study was to demonstrate that issues involved with tissue tolerance of a Resilon-containing sealer, RealSeal Sealer, cannot be attributed to its primer content.
URI: http://hdl.handle.net/10923/910
DOI: 10.1590/S1678-77572011000100011
ISSN: 1678-7757
Aparece en las colecciones:Artigo de Periódico

Ficheros en este ítem:
Fichero Descripción TamañoFormato 
JAOS 2011 Grecca et al.pdfTexto Completo873,11 kBAdobe PDFAbrir
Ver


Todos los ítems en el Repositorio de la PUCRS están protegidos por derechos de autor, con todos los derechos reservados, y están bajo una licencia de Creative Commons Reconocimiento-NoComercial 4.0 Internacional. Sepa más.